PART1
1.Flash( Excessive flash)
2.Gate remnant
3.Short shot/shrinkage
4.Mould in dirt
5.Flow mark/white mark/ silver mark
6.Clamp mark
7.Foreign matter on/attached to product
8.Pin mark
9.Deformed
10.Moulding scratches

TO BE CONTINUED...
2#
 楼主| 发表于 2008-5-11 18:25:01 | 只看该作者
Part 2
11.color /paint smear
12.color /paint stains
13.Incompleted/uneven coverage
14.Color variation
15.Missing paint
16.Improper paint
17.Under/poor/over spraying
18.Coating peeling off/faded out
19.Uneven spraing
20.Painting scratched off
21.Incorrect color
22.Color migration
23.Color dismatch
24.Poor silk screening
25.Out of register
26.Poor registration
27.Paint blister
28.Insufficient paint
29.Solvent stain
30.Folwing Paint mark
3#
 楼主| 发表于 2008-5-11 18:32:55 | 只看该作者
Part 3
31.Loose Part/screw
32.Detached part
33.Wrong /poor/improper assembly
34.Excessive gap between two parts /parting line
35.Missing parts/accessories/instruction sheet
36.Misaligned assembly
37.Poor sonic welding
38.Under/incomplete welding
39.improper positioning
40.Shifted position

TO BE CONTINUED...
4#
 楼主| 发表于 2008-5-12 21:42:46 | 只看该作者
Part 4
41.Incomplete seam/stich
42.Missing sew-in label
43.Pleated/wrinkles
44.Open seam
45.Insufficient hair /plush
46.Uncutting/untrimmed thread end
47.Missed yarn
48.Broken Yarn/stitch
49.Long loose thread
50.Crease line in fabric
您需要登录后才可以回帖 登录 | 注册

本版积分规则

小黑屋|手机版|Archiver|外贸验货员网

GMT+8, 2025-1-25 07:41 , Processed in 0.035668 second(s), 18 queries , Gzip On.

Powered by Discuz! X3.2

© 2001-2013 Comsenz Inc.

快速回复 返回顶部 返回列表