验货员论坛

标题: 玻璃产品试摔标准? [打印本页]

作者: buweining    时间: 2010-5-24 21:56
标题: 玻璃产品试摔标准?
我想请教下各位同仁,所谓的玻璃制品摔箱测试具体是个什么样的国际标准,摔多高,几面。摔箱不计重量。
谢谢。。。。
作者: Kenny.li    时间: 2010-5-25 09:19


这个问题问的好啊


谁来解释下
作者: steven-1    时间: 2010-5-25 09:31
LZ有了发一份给我。我的邮箱是steven_7980@yahoo.com.cn
作者: damienwang    时间: 2010-5-25 15:57
1~20.99 lbs (0.45~9.54㎏)                           30 in /(76.20㎝)   
21~40.99 lbs(9.55~18.63㎏)                         24 in /(60.96㎝)   
41~60.99 lbs(18.64~27.72 ㎏)                        18 in /(45.72㎝)   
61~100 lbs  (17.73~45.45㎏)                        12 in /(30.48㎝)

Test procedure:
Drop 1: Most fragile corner or corner at mfg. Joint.
Drop 2: Shortest edge radiating from corner.
Drop 3: Next longest edge radiating from corner.
Drop 4: Longest edge radiating from corner.
Drop 5: Flat on one of the smallest faces
Drop 6: Flat on the opposite small face.
Drop 7: Flat on one of the medium faces.
Drop 8: Flat on the opposite medium face.
Drop 9: Flat on one of the largest faces.
Drop 10: Flat on the opposite large face.
作者: 操张生    时间: 2010-5-30 14:43
我现就是想更名
作者: 操张生    时间: 2010-5-30 14:45
版主
帮我更下名吧
作者: lgqqq28    时间: 2010-6-18 20:02
I don't you.If anyone know,i hope can share with!
作者: harrylee0    时间: 2010-8-30 16:52
4楼的只是通用摔箱标准
作者: peng325    时间: 2010-12-3 23:43
哈哈,WAL 好象就两个等级的